2021-11-22 10:32| 發(fā)布者: steelfu4mo| 查看: 1098| 評論: 0 |原作者: 佛山萬慶物資
佛山市萬慶物資有限公司在10余年的彩鋼卷銷售過程中,不斷的接到客戶提到的關(guān)于彩鋼板的各種各樣的問題。當(dāng)然一些比較復(fù)雜的問題是無法用文字來表達(dá)的,只能通過電話溝通的方式解決。這也就是常碰到客戶發(fā)信息問我們的時候,而我們需要問客戶電話,打電話給客戶的重要原因。
Foshan Wanqing Materials Co., Ltd. In more than 10 years of color steel volume sales process, constantly received customers mentioned about a variety of problems about color steel plate.Of course, some of the more complex problems can not be expressed in words, and can only be solved through telephone communication.That is the important reason why we often encounter a customer to send a message to ask us, and we need to ask the customer phone and call customers.
相信彩涂板的面漆的問題困擾了不少人許久,那為什么總會遇到彩涂板掉漆呢?
Believe that the problem of color paint has troubled many people for a long time, then why always encounter color board paint?
彩涂板的面漆又分為面漆種類、面漆厚度、烘烤時間。面漆種類可分為:普通PE聚酯面漆(一般用),PVDF氟碳樹酯面漆(化工用),SMP聚酯面漆(而溫,耐磨用),HDP高耐候樹酯面漆(海洋氣候環(huán)境外用),HPC自清潔面漆(粉塵污染用),抗菌聚酯面漆(醫(yī)療潔凈環(huán)境用)。
The paint of color coating board is divided into types of paint, paint thickness and baking time.The types of paint can be divided into: general PE polyester paint (general), PVDF fluorocarbon paint (for chemical), SMP polyester paint (while temperature, wear resistant), HDP high resistant tree ester paint (for Marine climate environment), HPC self-cleaning paint (dust pollution), antibacterial polyester paint (for medical clean environment).
除了面漆種類就是面漆厚度了,不管哪種面漆種類,要達(dá)到品質(zhì)要求必須要達(dá)到一定的涂膜厚度,大鋼廠彩涂板,正面漆一般在18-25um,反面漆一般在8-15um。就像人穿衣服一樣,只有把面漆的厚度做足了才能充分抵御外來環(huán)境的侵蝕。再一次就是烘烤時間了,當(dāng)面漆種類很好,面漆膜厚達(dá)到,如果烘烤時間不夠,面漆就很容易產(chǎn)生粉化和脫落。大鋼廠烘箱比小廠一般都要長50-200米。
In addition to the type of paint is paint thickness, no matter which kind of paint, to achieve quality requirements must reach a certain coating thickness, large steel color plate, front paint is generally in 18-25um, reverse paint is generally in 8-15um.Just like people wear clothes, only the thickness of the face paint can fully resist the erosion of the external environment.Once again is the baking time, the face to face paint type is very good, the face paint film thickness is reached, if the baking time is not enough, the face paint is easy to produce powder and fall off.Large steel mill ovens are generally 50-200 meters longer than small factories.
還有就是很多的客戶把彩鋼卷運到加工廠后,一壓制成型就掉漆,或者是把漆面括花,這一般就是壓制方式不對,或是鋼卷面漆烘烤時間不夠,主要原因一般在設(shè)備上,有的設(shè)備差,滾輪上有很多的毛刺。
There is also a lot of customers after the color steel roll to the processing plant, a suppression molding on the paint, or the paint bracket, this is generally the suppression way is wrong, or the steel coil paint baking time is not enough, the main reason is generally in the equipment, some equipment is poor, there are a lot of burrs on the wheel.
很多工程在彩鋼板安裝的時候,出現(xiàn)工人不小心用利器劃傷面漆,或是在鋼板大小不一進(jìn)行切割的時候,有紅熱的切割鐵屑掉到面漆上,對面漆產(chǎn)生燒灼破壞。彩鋼板的面漆本身是一個整體的,如果局部出現(xiàn)劃傷,或是燒灼,那就會以點代面的出現(xiàn)紅銹,穿孔,最后大面積的生銹漏雨。還有一個不可避免的就是鉚釘,鉚釘必定會打穿鋼板,讓彩鋼板現(xiàn)現(xiàn)切面,經(jīng)過雨水流過形成銹蝕。
A lot of projects in the installation of color steel plate installation, workers accidentally scratch the paint with sharp tools, or in the size of the steel plate is different, there are red hot cutting iron chips fell to the paint, the opposite paint produces burning damage.The surface paint of the color steel plate itself is a whole, if the local scratches, or burning, it will replace the surface of red rust, perforation, and finally a large area of rust leakage.There is an inevitable is the rivet, rivevet will break through the steel plate, let the color steel plate now cut, through the rain to form rust.
佛山市萬慶物資有限公司作為彩涂板行業(yè)的一員,我們一直在孜孜不倦的努力推廣彩涂鋼板的好處以及高性能彩涂鋼板。佛山萬慶公司彩涂鋼板具有良好的加工性能,正常使用環(huán)境下,漆膜完整性保持10年以上。
Foshan Wanqing Materials Co., Ltd. As a member of the color coating plate industry, we have been working hard to promote the benefits of color coating steel plate and high-performance color coating steel plate.Foshan Wanqing Company painted steel plate has good processing performance. Under the normal use environment, the integrity of the paint film has been maintained for more than 10 years.